logo
Wuhan Fengfan International Trade Co.,Ltd. 86-27-85615818 info@fengfan.net
Cyanide Zinc Plating Chemicals Bright Zinc Process Brightener 96

Cyanide Zinc Plating Chemicals Bright Zinc Process Brightener 96

  • Menyoroti

    Cyanide Zinc Plating Chemicals

    ,

    Cyanide Zinc Process Brightener

    ,

    Zinc Process Brightener 96

  • barang
    bahan pembantu kimia
  • Menggunakan
    Pelapisan seng
  • Jenis
    Pembersih Elektroplating
  • Fitur
    Pelapisan seng sianida
  • Tempat asal
    Cina
  • Nama merek
    FENG FAN
  • Nomor model
    Pencerah 96
  • Kuantitas min Order
    Bisa dinegosiasikan
  • Harga
    dapat dinegosiasikan
  • Kemasan rincian
    Kemasan standar ekspor
  • Waktu pengiriman
    15-25 hari kerja
  • Syarat-syarat pembayaran
    L/C, D/A, D/P, T/T, Western Union, MoneyGram
  • Menyediakan kemampuan
    200000pcs/hari

Cyanide Zinc Plating Chemicals Bright Zinc Process Brightener 96

Brightener 96 for Cyanide Zinc plating

 

 

PROPERTIES

 

 

1. Wide bright area, bright deposit can be obtained when current density is 0.2~2A/dm2.

2. Strong throwing power, uniform bright deposit can be obtained on the complex parts, especially suitable for barrel plating.

3. Suitable for low-chrome passivating, it can lower pollution over 90% comparing with traditional Cr6+ pollution.

4. Suitable for high, medium and low cyanide plating bath.

5. It doesn’t contain aldehyde, it is stable and has low consumption in strong alkaline solution.

 

 

BATH INSTRUCTION

 

 

  Low cyanide Medium cyanide High cyanide Little cyanide
ZnO 10~15g/L 15~25g/L 35~45g/L 11~12g/L
NaCN 15~20g/L 25~40g/L 70~90g/L 6~10g/L
NaOH 70~80g/L 70~80g/L 80~100g/L 110~120g/L
Na2CO3 15~20g/L 15~20g/L 15~20g/L  
Na2S       0.1~0.3g/L
Brightener 96 5m/L 5m/L 5m/L 5m/L
Anode material 1# pure zinc 1# pure zinc 1# pure zinc 1# pure zinc

 

 

 

TECHNICAL PROCESS:

 

 

Acidic degreasing and derusting → rinse → alkaline chemical degreasing → hot-water washing → flowing cool water washing → activate(10%HCl) → rinse → bright zinc plating → recycle → rinse → neutralization (2~3% HNO3) → low-chrome passivation → rinse → drying (60~80ºC)

 

 

BRIGHTENER REPLENISHING:

 

 

1. On the natural working condition, when temperature range is 23~43ºC, brightener consumption is 100~150ml/KAH.

 

  2. Replenishing brightener little and normally, when barrel plating, replenishing it within half an hour before leaving bath, it can assure stable quality and low brightener consumption.